I learned something new today...
|
|
11-02-2011, 09:09 PM
Post: #1
|
|||
|
|||
|
I learned something new today...
... today I learned to look at other parts of the concrete design. The slab design said 5". But, one side of the gym came in at 99%.
I freaked out and said oh no oh no henny penny the sky is falling. I now feel pretty dumb. After some research the GC pointed out that the side of the gym that is reading high has a masonry wall. On that side of the room, the concrete is 14" thick to support the masonry wall. So duh it isn't dry. Anyway, I have to figure out how to read walls now before bid. Not sure how but I will have to pull out this projects plans and teach myself a new skill. Learn something new every day. Shows why we have GC's. They do have the whole building in mind. Now I have to find out if the sealing company can do the whole bead blast and seal and top coat 12' of concrete without having to level the whole floor. |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
I learned something new today... - eaadams - 11-02-2011 09:09 PM
RE: I learned something new today... - CC Solutions - 11-03-2011, 06:50 AM
|



Help
Advanced Search



![[-] [-]](images/collapse.gif)