false high test results
|
|
10-28-2011, 02:03 PM
Post: #11
|
|||
|
|||
RE: false high test results
(10-28-2011 11:47 AM)CC Solutions Wrote: The proper procedure is to vac the hole, scrub it with a wire brush, vac and repeat until the hole is clean. Clean = no dust. I honestly must disagree. Shoving anything that tight causing friction against the wall of the hole has got to create some more dust at the bottom of the hole. Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|
10-28-2011, 02:12 PM
Post: #12
|
|||
|
|||
RE: false high test results
(10-28-2011 02:03 PM)Ernesto Wrote:(10-28-2011 11:47 AM)CC Solutions Wrote: The proper procedure is to vac the hole, scrub it with a wire brush, vac and repeat until the hole is clean. Clean = no dust. Well you did brush it out! JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|