(10-28-2011 11:47 AM)CC Solutions Wrote:  The proper procedure is to vac the hole, scrub it with a wire brush, vac and repeat until the hole is clean. Clean = no dust.

I honestly must disagree. Shoving anything that tight causing friction against the wall of the hole has got to create some more dust at the bottom of the hole.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
10-28-2011, 02:12 PM
Post: #12
RE: false high test results
(10-28-2011 02:03 PM)Ernesto Wrote:  
(10-28-2011 11:47 AM)CC Solutions Wrote:  The proper procedure is to vac the hole, scrub it with a wire brush, vac and repeat until the hole is clean. Clean = no dust.

I honestly must disagree. Shoving anything that tight causing friction against the wall of the hole has got to create some more dust at the bottom of the hole.

Well you did brush it out!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious