Understood, JD. I'm still getting used to the dynamics of universal standards, how they are set, and how manufacturers respond and to what level they are involved.

The way I see it, the standards should set a "starting point" for methods and levels, and the manufacturers should have the option of setting their warranty levels based on their own research with the standards used as a cross-reference.

Here, Most of the folks involved in developing the standards agree that the manufacturers should set their levels, but are not convinced they've done enough of their own research, and are simply copying what's done elsewhere. Mind you, since the US seems to be way ahead of us, bouncing off some of your manufacturer levels is not a stupid idea. Many of the products and technology are US sourced anyway.

Pat Atherton
Floor Test Australia
www.moisturetesting.com.au

"Democracy ... can only exist until the majority discover they can vote themselves largess out of the public treasury" - Tytler, De Tocqueville, Reagan
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Ambient humidity vs. RH - Rubensgt40 - 10-04-2011, 09:29 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-06-2011, 06:41 AM
RE: Ambient humidity vs. RH - Ernesto - 10-06-2011, 03:43 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-06-2011, 05:16 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-06-2011, 06:43 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-06-2011, 09:20 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-07-2011, 06:07 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-08-2011, 12:24 AM
RE: Ambient humidity vs. RH - Ernesto - 10-08-2011, 01:42 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-09-2011, 12:58 AM
RE: Ambient humidity vs. RH - eblakewi - 10-10-2011, 11:21 AM
RE: Ambient humidity vs. RH - CC Solutions - 10-10-2011, 11:37 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-10-2011, 02:53 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-10-2011, 03:47 PM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-11-2011, 04:32 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-12-2011, 06:15 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-13-2011, 09:12 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-14-2011, 06:12 AM
RE: Ambient humidity vs. RH - Rubensgt40 - 10-16-2011 02:42 PM
RE: Ambient humidity vs. RH - CC Solutions - 10-16-2011, 06:09 PM