Yes CMoore, there are too many problems with it, and manufacturers are realizing that a proper CaCl test can be conducted and good numbers harvested yet the floor may have moisture related problems in the future.
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|