Can tape over the probe cause erroneous readings?
10-12-2011, 06:50 PM
Post: #3
RE: Can tape over the probe cause erroneous readings?
(10-12-2011 04:07 PM)eaadams Wrote:  I think it would do the same thing as putting a puddy on the sleeve to hold it in place.

I am unsure if they affect anything, perhaps do a few side by side tests on some jobs?

You mean like a puddy cat? Big Grin

I'm sure it doesn't have an effect on a 72 hour reading, but how about a 4 month test? I think anything suppressing the natural release of moisture form the slab would be of concern...