Can tape over the probe cause erroneous readings?
10-04-2011, 04:00 PM
Post: #1
Can tape over the probe cause erroneous readings?
Do you think duct tape over the probe cap will cause erroneous readings?
I am believing it can so I have quit doing this. I used to put a piece of duct tape over the cap to keep the dang cap in place because you know how people love to rip that cap off and fill the hole with dirt! Dodgy

But I think the tape will cause the slab to dry more slowly than it normally would. So I won't use tape on a long term test.

Thoughts?

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
10-12-2011, 04:07 PM
Post: #2
RE: Can tape over the probe cause erroneous readings?
I think it would do the same thing as putting a puddy on the sleeve to hold it in place.

I am unsure if they affect anything, perhaps do a few side by side tests on some jobs?
Find all posts by this user
Quote this message in a reply
10-12-2011, 06:50 PM
Post: #3
RE: Can tape over the probe cause erroneous readings?
(10-12-2011 04:07 PM)eaadams Wrote:  I think it would do the same thing as putting a puddy on the sleeve to hold it in place.

I am unsure if they affect anything, perhaps do a few side by side tests on some jobs?

You mean like a puddy cat? Big Grin

I'm sure it doesn't have an effect on a 72 hour reading, but how about a 4 month test? I think anything suppressing the natural release of moisture form the slab would be of concern...

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
10-12-2011, 06:54 PM
Post: #4
RE: Can tape over the probe cause erroneous readings?
I wonder if that big pile of drywall gets moisture on the bottom....
Find all posts by this user
Quote this message in a reply
06-25-2012, 11:38 PM (This post was last modified: 06-25-2012 11:39 PM by eaadams.)
Post: #5
RE: Can tape over the probe cause erroneous readings?
Well I have two testers doing this now. I have not seen a difference. I have seen one set of tests start around 99 and they got down to the low 90's

edit ....

over three months
99 to 86
94 to dead probe
90 to 80
99 to 90
96 to 81
99 to 85
99 to 91
99 to 85
Find all posts by this user
Quote this message in a reply
06-26-2012, 05:52 AM
Post: #6
RE: Can tape over the probe cause erroneous readings?
Very interesting.

I need to find out how Wagner has redesigned the test probes now that the requirement for a full sleeve is in effect. The previous probes would breathe, they have holes in them, but are they designed to breathe a certain percentage to mimic porous concrete?

If they allow moisture to escape from the test hole, how will 3 month old tests correlate with new tests? Huh

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
07-01-2012, 04:57 AM
Post: #7
RE: Can tape over the probe cause erroneous readings?
Interesting stuff.

Because of problems I've had with sensor contamination or flat out destruction (from water) after placement, I caulk the orange caps after initial place AND cover the caps with bright color tape. I also use a marker and write "TEST IN PROGRESS DO NOT DISTURB" on the tape. I also ask the GC to ask workers to do their best to not disturb my test locations. This seems to work, but I never thought of the tape having an adverse affect on my results.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Visit this user's website Find all posts by this user
Quote this message in a reply
07-01-2012, 08:42 AM
Post: #8
RE: Can tape over the probe cause erroneous readings?
I have not tested or seen test results regarding the taping of sensor caps. I have seen test sights with several pieces of duct tape placed over the caps and I would suspect that this would be an issue on long term testing.

The concrete needs to emit vapor to dry. Any barrier to emissions will create an abnormally high reading area (such as an area where pallets of materials were stacked for several months). We know moisture vapor doesn't travel sideways through a slab, so I wonder how much a small amount of tape, say 4" by 6" over the sensor, could effect the reading.

My gut feeling is that it could throw it off quite a bit on long term testing.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
07-01-2012, 09:09 AM
Post: #9
RE: Can tape over the probe cause erroneous readings?
Would be helpful to hear what Ray Thompson says.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Visit this user's website Find all posts by this user
Quote this message in a reply
07-03-2012, 12:44 PM
Post: #10
RE: Can tape over the probe cause erroneous readings?
No, It doesn't matter if you put tape over the hole or not
The reading is at the 40% depth and not the gradient of the hole.
Rayt
Find all posts by this user
Quote this message in a reply