Using compressed air to clean out the concrete hole.
|
|
10-07-2011, 06:35 PM
Post: #9
|
|||
|
|||
RE: Using compressed air to clean out the concrete hole.
(10-07-2011 04:01 PM)rapidrhrep Wrote: Well, I guess the all knowing rapidrh experts are not going to chime in on this one or my question about static electricity. sigh Well thanks there ole buddy...Jason I mean. I think the standard says not to because ya might get s--t in yer eye and they don't want to be sued.
Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|