I have always told clients ...your slab is like a sponge. And yes, I do see my kitchen sponge curl up when it drys out. Howard and I desperately need to talk. But that Ron guy always gets in the way. It's like Ron is his personal security secretary.
Yeah sure Howard has more better....yes more better people to talk to or things to do than talk to little oh me, the installer from Tucson. But I could tell him a thing or three about concrete down here no one else knows about cept for maybe Bob. Now that would be a power lunch, me Bob and Howard. Course you guys would be invited as well.Bring your golf clubs. Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|
02-14-2011, 11:26 PM
Post: #12
|
|||
|
|||
|
RE: Was on a job yesterday....
Hah yea right. Guess I will see you at woc 2012 then.
|
|||
|
02-15-2011, 07:52 AM
(This post was last modified: 02-15-2011 07:53 AM by Ernesto.)
Post: #13
|
|||
|
|||
|
RE: Was on a job yesterday....
Why would I go to http://woc2012.org/woc_2012.html ? Thats way to far and expensive for me.
![]() First I would tell him most all the slabs here are crowned not concave. ( must be on the opposite side of the world) I'm always running into humps in the middle of rooms. Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|
10-01-2011, 05:32 AM
Post: #14
|
|||
|
|||
RE: Was on a job yesterday....
(10-01-2011 04:14 AM)kathleen14maali Wrote: its very unfortunate to blame Howard. These spammers crack me up!!! But they know how to attach pictures to their user file... Something I can't figure out....
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
10-03-2011, 08:59 AM
Post: #15
|
|||
|
|||
|
RE: Was on a job yesterday....
Thanks JD. we've removed the spam and spammer
|
|||
|
10-03-2011, 09:07 AM
Post: #16
|
|||
|
|||
RE: Was on a job yesterday....
(10-03-2011 08:59 AM)admin Wrote: Thanks JD. we've removed the spam and spammer Why blame everything on Howard???
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|



Help
Advanced Search




![[-] [-]](images/collapse.gif)