Successful floor repair after failure!
|
|
09-29-2011, 08:42 PM
(This post was last modified: 09-29-2011 08:44 PM by eaadams.)
Post: #15
|
|||
|
|||
|
RE: Successful floor repair after failure!
Our preferred asbestos abatement sub uses IR to remove the tiles then they high pressure wash. The chemical strippers are not worth it. Compared to the IR, it is like going from soft to hardwood. Different world.
Speaking of silicates, beware, I know of a few schools where the silicate contamination is SO bad that we are having to HAZMAT all the waste water. Of course, both of the above in California are so we sub it all out. Not worth the liability risk. |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|