Self consolidating concrete (SCC)
09-29-2011, 08:29 AM
Post: #6
RE: Self consolidating concrete (SCC)
Good question Stephen, I've never seen it. It has to be expensive!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
RE: Self consolidating concrete (SCC) - CC Solutions - 09-29-2011 08:29 AM