SSC concrete is a low w/c ratio highly plasticized concrete. It is amazing how it flows and yet the coarse aggregate still remains suspended. The heavy pours do not need to be vibrated like normal concrete. It does dry faster than normal concrete because of the low w/c ratio and less water.