(09-28-2011 06:20 AM)CC Solutions Wrote: We clean concrete in hospitals where the sheetrock is on the floor. We use a 4,000 psi pressure washer and a rotating scrubber and water blast the floor! We even spray down the lower half of the walls! Then we squeegee up the water, vacuum up everything we can and immediately apply a water borne epoxy to the concrete. You have no clue about the difference in residential and commercial work do you? Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|