(09-26-2011 06:16 PM)CC Solutions Wrote: Yes, they are used all the time, especially to remove asbestos enriched adhesive. I've inspected a couple of floors where stripper...the orange oil stuff was used to remove cutbac adhesives then a wood floor glued to the slab. Turned into a floater real quick! On one of them the enduser contracted out the company because the box store told them it needed to be removed prior to installation and they would not do it. The box store got away with it because they didn't put the stripper on. I thought they should have done a bond test first but we all know they never do that kinda stuff.
Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|