How are you addressing cracks?
|
|
09-14-2011, 07:09 PM
Post: #21
|
|||
|
|||
|
RE: How are you addressing cracks?
There's the ole saying. "Honor the joint". Can't tell ya how many of those I've seen. Thats why I would never fill it with concrete. The ceramic tile industry has addressed this.
Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|