50% fail rate
|
|
09-12-2011, 05:43 PM
Post: #6
|
|||
|
|||
|
RE: 50% fail rate
Revisiting this thread and I was just thinking that if the probes were cold and put into a warm slab there could be condensation forming on the sensor which will mess with readings.... Typically this is something we need to worry about in the north, not so much in southern climes.
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
50% fail rate - eaadams - 05-27-2011, 10:55 AM
RE: 50% fail rate - admin - 05-27-2011, 03:55 PM
RE: 50% fail rate - eaadams - 05-27-2011, 04:57 PM
RE: 50% fail rate - CC Solutions - 05-30-2011, 11:18 AM
RE: 50% fail rate - eaadams - 05-30-2011, 01:24 PM
RE: 50% fail rate - CC Solutions - 09-12-2011 05:43 PM
RE: 50% fail rate - eaadams - 09-13-2011, 03:07 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 05:44 PM
RE: 50% fail rate - eaadams - 09-13-2011, 05:50 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 05:58 PM
RE: 50% fail rate - eaadams - 09-13-2011, 06:01 PM
RE: 50% fail rate - CC Solutions - 09-13-2011, 06:04 PM
|