(08-26-2011 02:30 PM)CC Solutions Wrote: If a crack hasn't moved in a month, after I seal the slab it may very well move later! The slab has been drying out the top, the top has shrunk, and the slab is most likely curled a bit and raised at the control joints. When I epoxy that slab the moisture will redistribute and the slab will relax and un-curl a bit. If there is any patch in those control joints it will be squished out. I don't want my self-leveler in the joints and cracks because I am really going to rock the slab's world and it is going to probably change because of what I do. "Fill it with cement, epoxy over it to seal it well, and put flooring on it. It will hold up" So I am confused. You put cement in the crack not your self leveler then you epoxy over it / patch then put flooring on top. Seems like a contradiction. |
|||
|