Epoxy over 7 day old slab
|
|
08-21-2011, 08:13 AM
Post: #11
|
|||
|
|||
|
RE: Epoxy over 7 day old slab
Thanks again JD. gene
|
|||
|
08-25-2011, 11:01 AM
Post: #12
|
|||
|
|||
RE: Epoxy over 7 day old slab
(08-21-2011 08:06 AM)CC Solutions Wrote: Koster and Ardex are my two main products. I did a Koster job Thursday and an Ardex job Saturday. I had a chance to use the newish Ardex MC Rapid. Weird stuff for sure. Filled with metallic specs which are supposed to help provide the barrier layer. For the MC Rapid, we are installing today a job over our local Levelmaster Elite favorite surface prep guy and the sealer he used they said has graphite in it. We saw some shiny reflective black where the Feather Finish was a little thin. It must have been this MC Rapid product. I'd like to know EVERYTHING you can tell me about that product. It is true about the Levelmaster Elite. Very few get there and some have fallen off over time because it is expensive. However, I love to tell attorneys "this should be done by a Levelmaster Elite". It gives them a standard that I don't have to justify. Aquafin is a significant player in the North East & New England. They have been trying to make inroads in California. However, after their sales pitch was that they will sell to anyone... I walked away ... with haste. |
|||
|
08-25-2011, 04:39 PM
Post: #13
|
|||
|
|||
|
RE: Epoxy over 7 day old slab
I can tell you the MC Rapid stinks something fierce!!!! You wouldn't want to spread a bunch out in an operating hospital.... (like I did
).
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
08-26-2011, 02:03 PM
Post: #14
|
|||
|
|||
|
RE: Epoxy over 7 day old slab
Whattype of epoxy? Amid-based or amine-based?