Self-leveling concrete - My bonehead mistake
08-26-2011, 01:59 PM
Post: #11
RE: Self-leveling concrete - My bonehead mistake
try a barrel of water with blocks of ice to cool the water.
watch the four temperatures; water, powder, ambient and slab. The cooler the better, but not below 50 degrees
Rayt
Find all posts by this user
Quote this message in a reply
08-26-2011, 02:36 PM
Post: #12
RE: Self-leveling concrete - My bonehead mistake
I should make a cooling coil to drop in a barrel of ice.... Like I have for cooling beer wort!

I bet 100' of 1/2" copper coiled up with a garden hose fitting on each end and then dropped into a barrel of ice would chill the flowing water just fine.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
08-26-2011, 03:24 PM
Post: #13
RE: Self-leveling concrete - My bonehead mistake
I know a long coil of tubing in a cooler of ice can keep beer cold for drinking. If you just use blocks of ice you can dip the cooled water out and add more as you need it. Many of the installers using self-levelers in the hot country will use 10 - 15 blockss of ice to chill their water. Try to keep the water temp below 70F. It doesn't have to be as cold, as does beer.
Rayt
Find all posts by this user
Quote this message in a reply
08-27-2011, 02:28 PM
Post: #14
RE: Self-leveling concrete - My bonehead mistake
Big Grin Big Grin Big Grin Big Grin
Quote this message in a reply
08-28-2011, 01:54 PM
Post: #15
RE: Self-leveling concrete - My bonehead mistake
Wow. Banned. I think that is the first person I saw banned!!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
08-28-2011, 02:34 PM
Post: #16
RE: Self-leveling concrete - My bonehead mistake
How does one get banned????? I know there are some that should be!
Rayt
Find all posts by this user
Quote this message in a reply
08-28-2011, 04:18 PM
Post: #17
RE: Self-leveling concrete - My bonehead mistake
You mean Admin doesn't give you the 'BAN' button? Wink

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
08-28-2011, 05:22 PM
Post: #18
RE: Self-leveling concrete - My bonehead mistake
Normally, when we ban someone for spamming, we delete any junk that they've posted... it looks like we missed that one.

@Ray - If you'd like to be able to ban people, let us know. In the past, we've tried to keep on top of the spammers so you don't have to worry about it.

- admin
Visit this user's website Find all posts by this user
Quote this message in a reply
08-28-2011, 06:46 PM
Post: #19
RE: Self-leveling concrete - My bonehead mistake
Oooo Oooo !!! Me Me!! Let me ban people!!!

It's part of my plan to take over the internet and then the world!!!! Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
08-28-2011, 07:13 PM
Post: #20
RE: Self-leveling concrete - My bonehead mistake
(08-28-2011 02:34 PM)rthompson Wrote:  How does one get banned????? I know there are some that should be!
Rayt

Uh oh JD! Big Grin I think he is talking about you. Tongue

Admin, anytime you give someone or trust somone mod clearence you should give them the button.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Visit this user's website Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious