Yes, broom finish it is Jason. Luckily my clients listen to me in which cases I have them buy a floater. Saves them tons of cash.
Now, if the hard troweled finish is not emitting, then I am golden doing a floating floor. Speaking of rubber. My buddy Bill at NRFS sent me to look at some rubber in a Sports Authority. I do trip hazard repairs and replacements for fortune 500 companies, any flooring. They have isles of rubber all over. Manager claims vendor ruined the rubber. Vendor uses a sizzor lift to change light bulbs. When he turned his wheels they scuffed the rubber. Looks like topical damage to the typical Joe, but what all it did was scuff the dirt off the top. The rubber in the whole place is filthy dirty. Managers says, it make it look like we have a dirty place.......lol It's so dirty you can hardly distinguish the white speckles in it. The scuff marks made the colors actually show up. Looking along the wall shelving that over hangs the rubber, you can see nice clean virgin rubber with all the color flecks. Manage wants the rubber replaced in front of the check out counters and some sections of isles. But that would look like day and night. The fix is worse than the remedy, well his remedy. My proposal is for him to clean the stinking rubber floor and the re-evaluate. Rubber ain't that easy to clean though. Now I've been there before to fix bubbles. Last time...bout a year ago I fixed twenty. Now they are all back and more. The bubbles run the length of the whole building in a straight line. Hmmm, wonder what that is from. ![]() To me having rubber glued down in a retail store is just crazy. Stephen Perrera dba Top Floor Installation Co. http://www.tucsonazflooring.com http://www.floorsavior.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Rhspec.com - Ernesto - 08-19-2011, 08:35 PM
RE: Rhspec.com - CC Solutions - 08-20-2011, 10:15 PM
RE: Rhspec.com - Ernesto - 08-21-2011, 08:25 AM
RE: Rhspec.com - CC Solutions - 08-21-2011, 08:38 AM
RE: Rhspec.com - Ernesto - 08-21-2011, 09:08 AM
RE: Rhspec.com - CC Solutions - 08-21-2011, 01:55 PM
RE: Rhspec.com - Ernesto - 08-21-2011, 04:29 PM
RE: Rhspec.com - dlpaal - 08-21-2011, 04:47 PM
RE: Rhspec.com - CC Solutions - 08-21-2011, 05:17 PM
RE: Rhspec.com - Ernesto - 08-21-2011, 05:38 PM
RE: Rhspec.com - CC Solutions - 08-21-2011, 05:40 PM
RE: Rhspec.com - Ernesto - 08-21-2011, 05:45 PM
RE: Rhspec.com - CC Solutions - 08-21-2011, 06:06 PM
RE: Rhspec.com - dlpaal - 08-21-2011, 06:27 PM
RE: Rhspec.com - Ernesto - 08-21-2011, 06:39 PM
RE: Rhspec.com - CC Solutions - 08-21-2011, 08:50 PM
RE: Rhspec.com - dlpaal - 08-21-2011, 09:40 PM
RE: Rhspec.com - Ernesto - 08-22-2011, 06:08 AM
RE: Rhspec.com - CC Solutions - 08-22-2011, 06:23 AM
RE: Rhspec.com - rapidrhrep - 08-22-2011, 11:43 AM
RE: Rhspec.com - Ernesto - 08-22-2011 04:42 PM
RE: Rhspec.com - CC Solutions - 08-22-2011, 09:19 PM
RE: Rhspec.com - Ernesto - 08-23-2011, 08:16 AM
RE: Rhspec.com - Ernesto - 08-23-2011, 07:27 PM
RE: Rhspec.com - CC Solutions - 08-23-2011, 09:44 PM
RE: Rhspec.com - eaadams - 08-24-2011, 12:48 PM
RE: Rhspec.com - CC Solutions - 08-24-2011, 01:03 PM
RE: Rhspec.com - Ernesto - 08-24-2011, 07:13 PM
RE: Rhspec.com - eaadams - 08-25-2011, 10:42 AM
RE: Rhspec.com - CC Solutions - 08-25-2011, 04:35 PM
RE: Rhspec.com - james01 - 09-15-2011, 12:19 AM
RE: Rhspec.com - CC Solutions - 09-15-2011, 05:03 AM
RE: Rhspec.com - Adonis - 12-19-2011, 11:46 PM
|



Help
Advanced Search





![[-] [-]](images/collapse.gif)