Koster and Ardex are my two main products. I did a Koster job Thursday and an Ardex job Saturday. I had a chance to use the newish Ardex MC Rapid. Weird stuff for sure. Filled with metallic specs which are supposed to help provide the barrier layer.
It's funny how Ardex and Koster approach the same goal from completely different perspectives. Both companies are excellent. I have not used Aquafin but it seems to be a solid product with a good reputation. To be a Levelmaster Elite, you must be recommended by an Ardex rep and pass their tests. They don't let many become Elite, but anyone can buy Ardex products. Koster will not sell products to the public, you must go through their training. JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Epoxy over 7 day old slab - ec-Indy - 08-18-2011, 03:08 PM
RE: Epoxy over 7 day old slab - Ernesto - 08-18-2011, 07:30 PM
RE: Epoxy over 7 day old slab - ec-Indy - 08-18-2011, 10:29 PM
RE: Epoxy over 7 day old slab - CC Solutions - 08-19-2011, 07:07 AM
RE: Epoxy over 7 day old slab - Ernesto - 08-19-2011, 08:00 PM
RE: Epoxy over 7 day old slab - CC Solutions - 08-19-2011, 08:21 PM
RE: Epoxy over 7 day old slab - ec-Indy - 08-20-2011, 12:48 PM
RE: Epoxy over 7 day old slab - CC Solutions - 08-20-2011, 09:47 PM
RE: Epoxy over 7 day old slab - ec-Indy - 08-21-2011, 02:26 AM
RE: Epoxy over 7 day old slab - CC Solutions - 08-21-2011 08:06 AM
RE: Epoxy over 7 day old slab - ec-Indy - 08-21-2011, 08:13 AM
RE: Epoxy over 7 day old slab - eaadams - 08-25-2011, 11:01 AM
RE: Epoxy over 7 day old slab - CC Solutions - 08-25-2011, 04:39 PM
RE: Epoxy over 7 day old slab - rthompson - 08-26-2011, 02:03 PM
|



Help
Advanced Search


![[-] [-]](images/collapse.gif)