How are you addressing cracks?
08-19-2011, 08:26 PM
Post: #7
RE: How are you addressing cracks?
Yowsa!!! That one is going to cost some money to fix.... Oh wait, it may be big enough to pack hydraulic cement in the crack. I just used some stuff that comes in a pail, costs $30 and dries in 3 minutes!

Put it in a trench or hole that you find, and epoxy right over it.