Epoxy over 7 day old slab
|
|
08-19-2011, 08:21 PM
Post: #6
|
|||
|
|||
|
RE: Epoxy over 7 day old slab
I can think of 4 I trust for warranty. These four also have excellent technical departments. I have worked on projects where I have had to call the tech department of a less-than-4-star company and I was shocked at the unprofessionalism (7!!) that I heard...
The big companies are expensive, but not as expensive as crossing your fingers....
JD Grafton Concrete Answers for Flooring Problems JGrafton@ccsolves.com |
|||
|
« Next Oldest | Next Newest »
|
![]() |
|||||||
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |
|
| Messages In This Thread |
|
Epoxy over 7 day old slab - ec-Indy - 08-18-2011, 03:08 PM
RE: Epoxy over 7 day old slab - Ernesto - 08-18-2011, 07:30 PM
RE: Epoxy over 7 day old slab - ec-Indy - 08-18-2011, 10:29 PM
RE: Epoxy over 7 day old slab - CC Solutions - 08-19-2011, 07:07 AM
RE: Epoxy over 7 day old slab - Ernesto - 08-19-2011, 08:00 PM
RE: Epoxy over 7 day old slab - CC Solutions - 08-19-2011 08:21 PM
RE: Epoxy over 7 day old slab - ec-Indy - 08-20-2011, 12:48 PM
RE: Epoxy over 7 day old slab - CC Solutions - 08-20-2011, 09:47 PM
RE: Epoxy over 7 day old slab - ec-Indy - 08-21-2011, 02:26 AM
RE: Epoxy over 7 day old slab - CC Solutions - 08-21-2011, 08:06 AM
RE: Epoxy over 7 day old slab - ec-Indy - 08-21-2011, 08:13 AM
RE: Epoxy over 7 day old slab - eaadams - 08-25-2011, 11:01 AM
RE: Epoxy over 7 day old slab - CC Solutions - 08-25-2011, 04:39 PM
RE: Epoxy over 7 day old slab - rthompson - 08-26-2011, 02:03 PM
|