Cold Expansion Joint
08-09-2011, 10:02 PM
Post: #8
RE: Cold Expansion Joint
Oh, old slab! Well then moisture can be high in areas where the vapor retarder is compromised and pipes are broken, or any other number of things.

You'll have to ask an adhesive guru about the cutback.... Tongue

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com
Find all posts by this user
Quote this message in a reply
Post Reply 


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Cold Expansion Joint - eaadams - 08-08-2011, 11:12 AM
RE: Cold Expansion Joint - CC Solutions - 08-08-2011, 11:57 AM
RE: Cold Expansion Joint - eaadams - 08-08-2011, 01:42 PM
RE: Cold Expansion Joint - CC Solutions - 08-08-2011, 02:15 PM
RE: Cold Expansion Joint - eaadams - 08-09-2011, 09:28 PM
RE: Cold Expansion Joint - CC Solutions - 08-09-2011, 09:34 PM
RE: Cold Expansion Joint - eaadams - 08-09-2011, 09:55 PM
RE: Cold Expansion Joint - CC Solutions - 08-09-2011 10:02 PM
RE: Cold Expansion Joint - Ernesto - 08-14-2011, 08:23 PM
RE: Cold Expansion Joint - eaadams - 08-14-2011, 09:50 PM
RE: Cold Expansion Joint - CC Solutions - 08-15-2011, 04:04 AM
RE: Cold Expansion Joint - Ernesto - 08-16-2011, 08:11 PM
RE: Cold Expansion Joint - CC Solutions - 08-19-2011, 07:14 AM
RE: Cold Expansion Joint - eaadams - 10-21-2011, 06:53 PM
RE: Cold Expansion Joint - CC Solutions - 10-21-2011, 07:30 PM
RE: Cold Expansion Joint - eaadams - 10-21-2011, 07:49 PM
RE: Cold Expansion Joint - CC Solutions - 10-22-2011, 07:24 AM