Ph Of Concrete

#11
(02-26-2011, 12:10 AM)barry88rowe Wrote:  I have no idea why the pH in your influent water varies, I'd check environmental factors such as rainfall, temperature, and time of year for correlation.

Welcome Barry!!

Most of the concrete slabs we deal with will be either on grade with a vapor retarder below them or raised and poured in a pan. There should really be no influent moisture, only the original moisture included in the concrete mix. Temperature should be at service conditions.

Actually if you have incoming water, the PH is irrelevant! You have a real problem. Big Grin

If I'm off-base please don't be shy to say so! I get that a lot around here. Tongue
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
Ph Of Concrete - Ernesto - 02-16-2011, 05:17 PM
RE: Ph Of Concrete - CC Solutions - 02-18-2011, 10:46 AM
RE: Ph Of Concrete - Ernesto - 02-18-2011, 05:55 PM
RE: Ph Of Concrete - CC Solutions - 02-21-2011, 03:37 PM
RE: Ph Of Concrete - Ernesto - 02-22-2011, 08:10 PM
RE: Ph Of Concrete - CC Solutions - 02-23-2011, 10:14 AM
RE: Ph Of Concrete - Ernesto - 02-23-2011, 09:12 PM
RE: Ph Of Concrete - CC Solutions - 02-24-2011, 11:43 AM
RE: Ph Of Concrete - Ernesto - 02-24-2011, 07:40 PM
RE: Ph Of Concrete - barry88rowe - 02-26-2011, 12:10 AM
RE: Ph Of Concrete - CC Solutions - 02-26-2011, 07:29 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,321 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,097 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,096 11-08-2013, 01:41 PM
Last Post: eaadams
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 63,507 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,151 01-30-2013, 04:43 PM
Last Post: eaadams
  Self consolidating concrete (SCC) eaadams 32 59,852 05-08-2012, 07:04 AM
Last Post: CC Solutions
  World of Concrete 2012 eaadams 0 3,407 03-23-2012, 09:40 AM
Last Post: eaadams
  Old concrete slab moisture DeanC 23 50,233 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Self-leveling concrete - My bonehead mistake CC Solutions 37 65,197 09-20-2011, 10:07 AM
Last Post: CC Solutions
  Concrete Surface Texture eaadams 12 26,791 06-21-2011, 11:47 AM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)