Ph Of Concrete

#1
Got a question foir you Guru's out there.

Can the ph of the concrete tell you more about MVER's than any moisture test?
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply


Messages In This Thread
Ph Of Concrete - Ernesto - 02-16-2011, 05:17 PM
RE: Ph Of Concrete - CC Solutions - 02-18-2011, 10:46 AM
RE: Ph Of Concrete - Ernesto - 02-18-2011, 05:55 PM
RE: Ph Of Concrete - CC Solutions - 02-21-2011, 03:37 PM
RE: Ph Of Concrete - Ernesto - 02-22-2011, 08:10 PM
RE: Ph Of Concrete - CC Solutions - 02-23-2011, 10:14 AM
RE: Ph Of Concrete - Ernesto - 02-23-2011, 09:12 PM
RE: Ph Of Concrete - CC Solutions - 02-24-2011, 11:43 AM
RE: Ph Of Concrete - Ernesto - 02-24-2011, 07:40 PM
RE: Ph Of Concrete - barry88rowe - 02-26-2011, 12:10 AM
RE: Ph Of Concrete - CC Solutions - 02-26-2011, 07:29 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,374 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,198 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,188 11-08-2013, 01:41 PM
Last Post: eaadams
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 63,637 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,189 01-30-2013, 04:43 PM
Last Post: eaadams
  Self consolidating concrete (SCC) eaadams 32 60,078 05-08-2012, 07:04 AM
Last Post: CC Solutions
  World of Concrete 2012 eaadams 0 3,421 03-23-2012, 09:40 AM
Last Post: eaadams
  Old concrete slab moisture DeanC 23 50,380 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Self-leveling concrete - My bonehead mistake CC Solutions 37 65,337 09-20-2011, 10:07 AM
Last Post: CC Solutions
  Concrete Surface Texture eaadams 12 26,878 06-21-2011, 11:47 AM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)