Wagner vs GE Hygromaster, Please Coment
We are not accepting a 90-95% slab where product goes in at 80%.
The GC had an independent test with a GE Hygromaster and it read under 70%. What gives here? For fun, I took a calcium chloride test got a 3.61.
Whats wrong with the GE Hygromaster? Someone told me it did not satisfy the 2170?