PH TESTING

#4
(09-20-2010, 02:26 PM)CC Solutions Wrote:  PH and moisture will go hand in hand also.

I disagree. I have seen moisture results well below failure, low 80's%, but pH be in the 12 range (newer slabs). I have seen low pH and high moisture (old slabs).
Reply


Messages In This Thread
PH TESTING - MINUS - 09-02-2010, 10:04 AM
RE: PH TESTING - Ernesto - 09-03-2010, 08:11 AM
RE: PH TESTING - CC Solutions - 09-20-2010, 02:26 PM
RE: PH TESTING - hausenheimer - 07-22-2013, 07:07 AM
RE: PH TESTING - CC Solutions - 07-22-2013, 08:47 AM
RE: PH TESTING - hersitervery - 04-02-2014, 04:10 AM