(09-23-2008, 10:44 AM)Sam Bagley Wrote:  I’m fairly new at this. Is there a good method of determining the best locations to take my relative humidity measurements of the concrete slab?
Sam,
I use a topical moisture meter. I will find the high areas and place the probes there. If I do not have a toopical moisture meter i will try to establish a grid that gives me a good represntation of the entire area.