#10
How about a failing vapor retarder (they don't last forever) or a violation of the vapor retarder?

Either way it's a SERIOUS heads up that all is not well in moisture land.

By the way, when will you install the other 35 probes the ASTM requires?

Just kidding! Big Grin
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
99% RH in concrete slab - mwoody - 08-22-2010, 02:38 PM
RE: 99% RH in concrete slab - eaadams - 08-22-2010, 02:45 PM
RE: 99% RH in concrete slab - Ernesto - 08-22-2010, 09:42 PM
RE: 99% RH in concrete slab - mwoody - 08-23-2010, 05:54 AM
RE: 99% RH in concrete slab - eaadams - 08-23-2010, 09:17 AM
RE: 99% RH in concrete slab - mwoody - 08-27-2010, 07:24 AM
RE: 99% RH in concrete slab - eaadams - 08-27-2010, 11:33 AM
RE: 99% RH in concrete slab - Ernesto - 08-30-2010, 08:08 AM
RE: 99% RH in concrete slab - eaadams - 08-30-2010, 09:47 AM
RE: 99% RH in concrete slab - CC Solutions - 09-20-2010, 03:15 PM
RE: 99% RH in concrete slab - Floorguy - 02-03-2011, 12:55 PM
RE: 99% RH in concrete slab - eaadams - 02-03-2011, 01:53 PM
RE: 99% RH in concrete slab - Ernesto - 02-03-2011, 08:12 PM
RE: 99% RH in concrete slab - CC Solutions - 02-06-2011, 11:31 AM
RE: 99% RH in concrete slab - eaadams - 02-06-2011, 05:49 PM
RE: 99% RH in concrete slab - CC Solutions - 02-07-2011, 09:37 AM
RE: 99% RH in concrete slab - mwoody - 02-07-2011, 11:02 AM
RE: 99% RH in concrete slab - CC Solutions - 02-07-2011, 11:07 AM
RE: 99% RH in concrete slab - Ernesto - 02-14-2011, 08:37 PM
RE: 99% RH in concrete slab - CC Solutions - 02-14-2011, 09:06 PM
RE: 99% RH in concrete slab - eaadams - 02-14-2011, 11:22 PM
RE: 99% RH in concrete slab - Ernesto - 02-15-2011, 07:57 AM
RE: 99% RH in concrete slab - eaadams - 02-15-2011, 10:22 AM
RE: 99% RH in concrete slab - Ernesto - 02-15-2011, 11:43 AM
RE: 99% RH in concrete slab - CC Solutions - 02-15-2011, 03:43 PM
RE: 99% RH in concrete slab - Ernesto - 02-15-2011, 06:36 PM
RE: 99% RH in concrete slab - CC Solutions - 02-16-2011, 09:54 AM
RE: 99% RH in concrete slab - Ernesto - 02-16-2011, 05:13 PM
RE: 99% RH in concrete slab - CC Solutions - 02-18-2011, 10:11 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Determine Slab Thickness eaadams 1 5,694 06-20-2012, 03:07 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)