I've seen this in two instances. One where there was 2" of sand below slab and the vapor barrier and the sand never truly dried out. The other had 2" of sand and the gutter drains were being fed into the slab w/o a drain.
Reply


Messages In This Thread
99% RH in concrete slab - mwoody - 08-22-2010, 02:38 PM
RE: 99% RH in concrete slab - eaadams - 08-22-2010, 02:45 PM
RE: 99% RH in concrete slab - Ernesto - 08-22-2010, 09:42 PM
RE: 99% RH in concrete slab - mwoody - 08-23-2010, 05:54 AM
RE: 99% RH in concrete slab - eaadams - 08-23-2010, 09:17 AM
RE: 99% RH in concrete slab - mwoody - 08-27-2010, 07:24 AM
RE: 99% RH in concrete slab - eaadams - 08-27-2010, 11:33 AM
RE: 99% RH in concrete slab - Ernesto - 08-30-2010, 08:08 AM
RE: 99% RH in concrete slab - eaadams - 08-30-2010, 09:47 AM
RE: 99% RH in concrete slab - CC Solutions - 09-20-2010, 03:15 PM
RE: 99% RH in concrete slab - Floorguy - 02-03-2011, 12:55 PM
RE: 99% RH in concrete slab - eaadams - 02-03-2011, 01:53 PM
RE: 99% RH in concrete slab - Ernesto - 02-03-2011, 08:12 PM
RE: 99% RH in concrete slab - CC Solutions - 02-06-2011, 11:31 AM
RE: 99% RH in concrete slab - eaadams - 02-06-2011, 05:49 PM
RE: 99% RH in concrete slab - CC Solutions - 02-07-2011, 09:37 AM
RE: 99% RH in concrete slab - mwoody - 02-07-2011, 11:02 AM
RE: 99% RH in concrete slab - CC Solutions - 02-07-2011, 11:07 AM
RE: 99% RH in concrete slab - Ernesto - 02-14-2011, 08:37 PM
RE: 99% RH in concrete slab - CC Solutions - 02-14-2011, 09:06 PM
RE: 99% RH in concrete slab - eaadams - 02-14-2011, 11:22 PM
RE: 99% RH in concrete slab - Ernesto - 02-15-2011, 07:57 AM
RE: 99% RH in concrete slab - eaadams - 02-15-2011, 10:22 AM
RE: 99% RH in concrete slab - Ernesto - 02-15-2011, 11:43 AM
RE: 99% RH in concrete slab - CC Solutions - 02-15-2011, 03:43 PM
RE: 99% RH in concrete slab - Ernesto - 02-15-2011, 06:36 PM
RE: 99% RH in concrete slab - CC Solutions - 02-16-2011, 09:54 AM
RE: 99% RH in concrete slab - Ernesto - 02-16-2011, 05:13 PM
RE: 99% RH in concrete slab - CC Solutions - 02-18-2011, 10:11 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Determine Slab Thickness eaadams 1 5,688 06-20-2012, 03:07 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)