Adhesives and Moisture

#1
Food for thought:

A little tidbit I found in some lit:

302.2R-18 ACI COMMITTEE REPORT

"shown that the adhesive strength decreases with an increase
in the concrete’s MVER. When these tests were conducted,
however, there were no criteria for acceptable bond strength,
and scatter in the test results did not indicate a clear dividing line
between acceptable and nonacceptable adhesive bond strength.
A report on recent testing that attempted to correlate moisture
in the concrete with floor covering performance concluded
that: “The evidence presented suggests that there is no
relationship between the relative humidity of a concrete base
or screed and adhesion of resilient floor coverings” (The
Concrete Society 2004).
While moisture criteria are often used, the relationship
between these criteria and floor covering performance is not
well understood."
Reply


Messages In This Thread
Adhesives and Moisture - Ernesto - 02-03-2010, 01:41 PM
RE: Adhesives and Moisture - CC Solutions - 02-03-2010, 03:53 PM
RE: Adhesives and Moisture - Ernesto - 02-05-2010, 08:12 AM
RE: Adhesives and Moisture - CC Solutions - 02-05-2010, 11:56 AM
RE: Adhesives and Moisture - Ernesto - 02-17-2010, 03:32 PM
RE: Adhesives and Moisture - CC Solutions - 02-17-2010, 10:12 PM
RE: Adhesives and Moisture - Ernesto - 02-18-2010, 09:04 AM
RE: Adhesives and Moisture - CC Solutions - 02-18-2010, 09:34 AM
RE: Adhesives and Moisture - Ernesto - 02-18-2010, 03:19 PM
RE: Adhesives and Moisture - CC Solutions - 02-19-2010, 07:13 AM
RE: Adhesives and Moisture - Ernesto - 02-19-2010, 08:34 AM
RE: Adhesives and Moisture - CC Solutions - 02-19-2010, 11:07 AM
RE: Adhesives and Moisture - Ernesto - 02-19-2010, 05:31 PM
RE: Adhesives and Moisture - Ernesto - 03-08-2010, 03:11 PM
RE: Adhesives and Moisture - CC Solutions - 03-09-2010, 06:48 PM
RE: Adhesives and Moisture - Ernesto - 03-10-2010, 03:06 PM
RE: Adhesives and Moisture - CC Solutions - 03-18-2010, 06:31 PM
RE: Adhesives and Moisture - Ernesto - 03-19-2010, 06:01 PM
RE: Adhesives and Moisture - tbrown - 04-08-2010, 10:24 AM
RE: Adhesives and Moisture - CC Solutions - 04-08-2010, 08:10 PM
RE: Adhesives and Moisture - CC Solutions - 04-30-2010, 09:03 AM
RE: Adhesives and Moisture - CC Solutions - 05-01-2010, 09:40 AM
RE: Adhesives and Moisture - CC Solutions - 05-02-2010, 08:18 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Moisture going up Rubensgt40 3 1,550 07-05-2014, 03:18 AM
Last Post: Rubensgt40
  35-40 year old concrete with moisture problems Tscdad 13 7,331 05-19-2014, 10:55 AM
Last Post: eaadams
  Digital moisture meter QC worker 2 1,853 05-10-2014, 08:07 PM
Last Post: Rubensgt40
  Tandus removes moisture testing requirement eaadams 2 4,079 09-27-2013, 10:26 AM
Last Post: eaadams
  Carbide moisture testing CC Solutions 4 8,665 09-18-2012, 06:11 PM
Last Post: CC Solutions
  Old concrete slab moisture DeanC 23 50,546 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Flooring Manufacturer Warrenty in Relation to Moisture mwoody 5 10,916 08-14-2011, 08:43 PM
Last Post: Ernesto
Sad Is there a way to measure moisture plus cold temperatures sort of like a heat index b Ronald Edberg 4 10,718 07-01-2011, 07:11 PM
Last Post: rthompson
  Concrete Moisture Control Systems BuilderPDX 8 16,834 06-09-2011, 06:09 AM
Last Post: CC Solutions
  The Moisture Webinar Ernesto 17 33,286 04-01-2011, 09:02 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)