Bostik Ultra_Set Single Step says only dry to touch, no limits. Nothing about alkalinity/ph.
http://www.bostik-us.com/sites/default/files/ULTRA-SET_SingleStep.pdf

http://www.bostik-us.com/market-products/flooring/hardwood#singlestep