35-40 year old concrete with moisture problems
01-28-2014, 08:38 AM,
#4
RE: 35-40 year old concrete with moisture problems
It's very likely the vapor barrier has been compromised through deterioration. To verify, cut a section of floor out where the failures have occurred and check the condition of the vapor barrier. Depending on the aggressiveness of the soils, it is not uncommon that is 6 mill vapor barrier can deteriorate within 10 years.