article on testing

#3
I got a kick out of "Worse yet, the expansion joint between the slabs had no backer rod or sealant."

I had this happen on a job. No sealant at all. We pointed it out, they fixed it. Then they sued the contractor for a new floor. Made me sick

Oh yea and how'd I find it? I followed the ant trail. Ants always find a way
Reply


Messages In This Thread
article on testing - eaadams - 07-26-2013, 12:51 PM
RE: article on testing - CCR - 07-26-2013, 04:23 PM
RE: article on testing - eaadams - 07-26-2013, 05:51 PM
RE: article on testing - CC Solutions - 09-01-2013, 09:10 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  No Testing Requirements ???? CCR 3 5,140 06-28-2013, 10:26 AM
Last Post: eaadams
  Moisture Testing Awareness raised Down Under... Horror abounds... Rubensgt40 6 9,527 05-10-2013, 06:46 PM
Last Post: Rubensgt40
  insuti testing jim decker 27 26,727 05-02-2013, 12:31 PM
Last Post: jim decker
  How Do You Charge For Testing? CCR 23 22,496 03-21-2013, 05:05 PM
Last Post: CCR
  Another Great Ray Thompson Article eaadams 1 6,960 10-13-2012, 08:45 PM
Last Post: CC Solutions
  RH & CC Testing CCR 23 41,429 07-26-2012, 06:19 AM
Last Post: CC Solutions
  RH Testing For Parking Garages CCR 6 9,543 07-12-2012, 01:44 PM
Last Post: CCR
  Wagner Article Vapor Retarders eaadams 2 5,770 06-19-2012, 01:52 PM
Last Post: CC Solutions
  Wood Floor Testing eaadams 1 5,403 06-07-2012, 01:08 PM
Last Post: hnelson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)