Spec = I run away & dont bid
07-02-2013, 08:26 AM, (This post was last modified: 07-02-2013, 08:28 AM by CC Solutions.)
#3
RE: Spec = I run away & dont bid
Who wrote that spec??? Exclamation

It contradicts itself over and over! Sprayed on and troweled in, yet put on at 8-15 mils??? Flooring ready in 12 hours but troweled in?

And the mitigation has to not only provide a warranty for reducing the MVER and alkalinity, but a performance bond guaranteeing the concrete won't crack or delaminate?

You know what this is.... A project manager went through a few spec sheets and took verbiage from several manufacturers then shot for the moon and asked for a performance bond and a load of guarantees.

And you know what? Someone will bid it, bid it really low and get the job, then the thing will fail and they will walk away.

THAT is one guarantee I will stand by..... Wink

(06-27-2013, 12:36 PM)eaadams Wrote:  I got a kick out of this spec. Talk about unrealistic.


2. Subject to compliance with requirements, provide products indicated or equal products byone of the following:
a. Diamond Stone Products
b. Ardex Moisture Control


And Ardex would just LAUGH at this!!!
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Spec = I run away & dont bid - eaadams - 06-27-2013, 12:36 PM
RE: Spec = I run away & dont bid - CCR - 06-30-2013, 04:27 PM
RE: Spec = I run away & dont bid - CC Solutions - 07-02-2013, 08:26 AM
RE: Spec = I run away & dont bid - eaadams - 07-02-2013, 08:52 AM
RE: Spec = I run away & dont bid - CCR - 07-02-2013, 09:45 AM
RE: Spec = I run away & dont bid - eaadams - 07-02-2013, 10:27 AM
RE: Spec = I run away & dont bid - eaadams - 07-02-2013, 10:35 AM
RE: Spec = I run away & dont bid - CCR - 07-02-2013, 11:15 AM
RE: Spec = I run away & dont bid - eaadams - 07-02-2013, 11:17 AM
RE: Spec = I run away & dont bid - CCR - 07-02-2013, 12:06 PM