I think you should name the company. Otherwise others will not find this thread through google.

What I am surprised is he bid knowing this was in the mix. Out here on the left coast we've had more and more people just refuse to bid such projects in fear of the inevitable lawsuit because when you bid div Z you are forced to accept div C in the general conditions. So if you knew of the issue in div C pre-bid, you should have built in the repairs needed in div Z. Exp on private work where the bid is meaningless if you bid per plans and specs. Public work you have a right to qualify your bid but you still must stop the initial injury from happening if they cut you a contract before div C happens.
Reply


Messages In This Thread
Amazing Concrete Moisture Solution! - CCR - 05-30-2013, 05:33 PM
RE: Amazing Concrete Moisture Solution! - eaadams - 05-31-2013, 09:33 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Concrete doesn't crack eaadams 9 15,615 12-26-2012, 01:02 PM
Last Post: CC Solutions
  Light Weight Concrete on Pan Deck arlington 6 14,486 03-27-2012, 01:08 PM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)