Things like Agila are superplasticizers. So yes I agree with that caveat.

Slump as a Q/C is only good as Q/C for batch plant to site. It shouldn't be relied upon for performance.
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Kapow! Low RH by Sundt - eaadams - 05-06-2013, 09:42 PM
RE: Kapow! Low RH by Sundt - jim decker - 05-07-2013, 06:31 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 06:39 PM
RE: Kapow! Low RH by Sundt - jim decker - 05-07-2013, 06:54 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 07:24 PM
RE: Kapow! Low RH by Sundt - Rubensgt40 - 05-07-2013, 08:38 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 08:40 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-10-2013, 09:36 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-10-2013, 10:14 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-10-2013, 10:22 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-10-2013, 10:26 AM
RE: Kapow! Low RH by Sundt - rapidrhrep - 05-24-2013, 09:41 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-24-2013, 09:48 AM
RE: Kapow! Low RH by Sundt - rapidrhrep - 05-24-2013, 10:09 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-24-2013, 10:16 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-27-2013, 10:17 AM