Kapow! Low RH by Sundt
05-10-2013, 10:14 AM,
#9
RE: Kapow! Low RH by Sundt
Concrete slabs will dry at the rate of about 1" per month. So your 6" slab could dry in six months. We used to get those results consistently if we followed the guidelines.

Why is there air in the slab??? Is it outdoors? Subject to freezing?

I really like the LOW cement content of this slab.
When they spec less cement, they also use less water. Less water in = less water to dry out. Wink
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Kapow! Low RH by Sundt - eaadams - 05-06-2013, 09:42 PM
RE: Kapow! Low RH by Sundt - jim decker - 05-07-2013, 06:31 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 06:39 PM
RE: Kapow! Low RH by Sundt - jim decker - 05-07-2013, 06:54 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 07:24 PM
RE: Kapow! Low RH by Sundt - Rubensgt40 - 05-07-2013, 08:38 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 08:40 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-10-2013, 09:36 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-10-2013, 10:14 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-10-2013, 10:22 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-10-2013, 10:26 AM
RE: Kapow! Low RH by Sundt - rapidrhrep - 05-24-2013, 09:41 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-24-2013, 09:48 AM
RE: Kapow! Low RH by Sundt - rapidrhrep - 05-24-2013, 10:09 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-24-2013, 10:16 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-27-2013, 10:17 AM