Drilling test holes for depth confirmation

#2
I wish I knew how to answer that.

Same discussion brought up on this here thread

Although it did get a little off-track (for once not my fault JD Smile )

I don't think that the proximity of a narrow test hole to the probe location will be a big deal - but I have no scientific evidence to back that.

That said, I just did a test in a school where I hit re-bar three times before I finally got a successful probe hole. I will patch the dud holes up with some portland cement mix, but obviously not until after the readings are taken. I'm a little paranoid that the water in the patching mix will show up somewhere nearby...again, probably nothing scientific to back that but you can't be too careful.
The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher

Reply


Messages In This Thread
RE: Drilling test holes for depth confirmation - Rubensgt40 - 04-10-2013, 06:08 AM

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)