A byproduct of burning hydrocarbon fuels is moisture, so an improperly vented heating system can add moisture to the slab. However if fresh air is used for combustion this is usually not the case.

I tell people to begin testing slabs as soon as they can! I have installed RH probes in slabs and sealed the top with duct tape to keep water out of the probe when windows were still missing.

ATSM 2170 does have parameters to follow before RH tests are to be accepted as 'gospel' but the information gathered from early testing still has great value. Trending a slab's moisture content can help identify problems long before they become emergencies.

I'd rather tell a general that he needs to shot blast and bring in a dehumidifier system 3 months before he needs to put floor coverings down, than try to tell him that a week before he needs to start.....
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
When to Test - CFI - 11-22-2009, 11:36 AM
RE: When to Test - Ben - 11-24-2009, 12:23 PM
RE: When to Test - CC Solutions - 12-16-2009, 11:45 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Test Before You Spec! CCR 6 8,417 05-13-2013, 04:51 PM
Last Post: Ernesto
  Cal Chlor Test CCR 10 15,480 01-18-2013, 04:48 PM
Last Post: eaadams
  Another tester brought in to dispute test results. CC Solutions 4 9,691 08-14-2011, 09:32 PM
Last Post: CC Solutions
  Interesting Test Result eaadams 16 30,051 08-08-2011, 11:41 AM
Last Post: CC Solutions
  How to test RH levels after moisture barrier is used DShenk 3 10,624 08-30-2010, 12:42 PM
Last Post: Ernesto
  Old Slab Test eaadams 5 12,171 07-12-2010, 07:00 PM
Last Post: Ernesto
  pH test eaadams 2 7,879 07-09-2010, 09:45 AM
Last Post: eaadams
  Test time for RH test jigar0896 14 31,390 01-15-2010, 09:36 PM
Last Post: CC Solutions
  RH Test Hole Callout Ben 3 11,286 11-04-2008, 10:03 AM
Last Post: rthompson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)