RE: insuti testing
Vapor barrier or not, it seems to me RH testing is still the best testing option. Even with a quality barrier, finishers are still troweling new concrete too tight to let moisture escape. Literally every new slab I test is in the 90s. On big jobs, these slabs can be over 12 months old.
I'm in the midst of testing an interesting job with 2 different vapor barriers (6 mil and 15 mil) from well known manufacturers. In addition, concrete has 2 different finishes in different flooring areas (CSP 3-4 and slick, power-troweled). Testing will take place when the building is enclosed and conditioned. I can hardly wait to do this one.
JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
insuti testing - jim decker - 03-14-2013, 02:09 PM
RE: insuti testing - CCR - 03-16-2013, 04:41 PM
RE: insuti testing - jim decker - 03-17-2013, 07:49 PM
RE: insuti testing - CC Solutions - 03-19-2013, 06:41 AM
RE: insuti testing - jim decker - 03-19-2013, 09:35 AM
RE: insuti testing - CC Solutions - 03-19-2013, 08:38 PM
RE: insuti testing - jim decker - 03-20-2013, 07:42 AM
RE: insuti testing - CC Solutions - 03-21-2013, 11:50 AM
RE: insuti testing - CCR - 03-21-2013, 05:08 PM
RE: insuti testing - jim decker - 03-22-2013, 08:45 AM
RE: insuti testing - eaadams - 04-29-2013, 04:27 PM
RE: insuti testing - CC Solutions - 04-29-2013, 07:01 PM
RE: insuti testing - eaadams - 04-30-2013, 09:15 AM
RE: insuti testing - CC Solutions - 05-01-2013, 05:57 AM
RE: insuti testing - CCR - 05-01-2013, 06:16 AM
RE: insuti testing - CC Solutions - 05-01-2013, 06:24 AM
RE: insuti testing - rapidrhrep - 05-01-2013, 10:15 AM
RE: insuti testing - CCR - 05-02-2013, 03:42 AM
RE: insuti testing - CC Solutions - 05-02-2013, 05:53 AM
RE: insuti testing - CCR - 05-02-2013, 06:33 AM
RE: insuti testing - eaadams - 05-02-2013, 08:05 AM
RE: insuti testing - CC Solutions - 05-02-2013, 08:45 AM
RE: insuti testing - eaadams - 05-02-2013, 08:59 AM
RE: insuti testing - CC Solutions - 05-02-2013, 09:02 AM
RE: insuti testing - eaadams - 05-02-2013, 10:21 AM
RE: insuti testing - CC Solutions - 05-02-2013, 11:25 AM
RE: insuti testing - eaadams - 05-02-2013, 11:30 AM
RE: insuti testing - jim decker - 05-02-2013, 12:31 PM