insuti testing

#16
I always point out to clients that the flooring manufacturer requires an intact, proper and functioning vapor retarder directly under the concrete slab.

I also point out that even with a vapor retarder, there could be areas that were cut or punctured or joints that are wide open where moisture can get into the slab.

You can still read the RH, but if something is wrong that you can't see problems may arise later on.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
insuti testing - jim decker - 03-14-2013, 02:09 PM
RE: insuti testing - CCR - 03-16-2013, 04:41 PM
RE: insuti testing - jim decker - 03-17-2013, 07:49 PM
RE: insuti testing - CC Solutions - 03-19-2013, 06:41 AM
RE: insuti testing - jim decker - 03-19-2013, 09:35 AM
RE: insuti testing - CC Solutions - 03-19-2013, 08:38 PM
RE: insuti testing - jim decker - 03-20-2013, 07:42 AM
RE: insuti testing - CC Solutions - 03-21-2013, 11:50 AM
RE: insuti testing - CCR - 03-21-2013, 05:08 PM
RE: insuti testing - jim decker - 03-22-2013, 08:45 AM
RE: insuti testing - eaadams - 04-29-2013, 04:27 PM
RE: insuti testing - CC Solutions - 04-29-2013, 07:01 PM
RE: insuti testing - eaadams - 04-30-2013, 09:15 AM
RE: insuti testing - CC Solutions - 05-01-2013, 05:57 AM
RE: insuti testing - CCR - 05-01-2013, 06:16 AM
RE: insuti testing - CC Solutions - 05-01-2013, 06:24 AM
RE: insuti testing - rapidrhrep - 05-01-2013, 10:15 AM
RE: insuti testing - CCR - 05-02-2013, 03:42 AM
RE: insuti testing - CC Solutions - 05-02-2013, 05:53 AM
RE: insuti testing - CCR - 05-02-2013, 06:33 AM
RE: insuti testing - eaadams - 05-02-2013, 08:05 AM
RE: insuti testing - CC Solutions - 05-02-2013, 08:45 AM
RE: insuti testing - eaadams - 05-02-2013, 08:59 AM
RE: insuti testing - CC Solutions - 05-02-2013, 09:02 AM
RE: insuti testing - eaadams - 05-02-2013, 10:21 AM
RE: insuti testing - CC Solutions - 05-02-2013, 11:25 AM
RE: insuti testing - eaadams - 05-02-2013, 11:30 AM
RE: insuti testing - jim decker - 05-02-2013, 12:31 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
Wink article on testing eaadams 3 6,312 09-01-2013, 09:10 AM
Last Post: CC Solutions
  No Testing Requirements ???? CCR 3 5,188 06-28-2013, 10:26 AM
Last Post: eaadams
  Moisture Testing Awareness raised Down Under... Horror abounds... Rubensgt40 6 9,619 05-10-2013, 06:46 PM
Last Post: Rubensgt40
  How Do You Charge For Testing? CCR 23 22,713 03-21-2013, 05:05 PM
Last Post: CCR
  RH & CC Testing CCR 23 41,614 07-26-2012, 06:19 AM
Last Post: CC Solutions
  RH Testing For Parking Garages CCR 6 9,619 07-12-2012, 01:44 PM
Last Post: CCR
  Wood Floor Testing eaadams 1 5,426 06-07-2012, 01:08 PM
Last Post: hnelson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)