(04-29-2013, 04:27 PM)eaadams Wrote:  
(03-19-2013, 08:38 PM)CC Solutions Wrote:  No vapor retarder under concrete can end up being a disaster. Especially in buildings that are dehumidified often.

At world of Concrete Peter Craig said no vapor retarder invalidates the accuracy of RH testing. Scared the pants off of me.

If you think of why he said that it makes sense:

The RH probes are set at a depth where the RH measured will be the same today as it will be when the slab equilibrates.

With no vapor retarder, the moisture level is unlimited, so you cannot predict what it will be in the future. Wink
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
insuti testing - jim decker - 03-14-2013, 02:09 PM
RE: insuti testing - CCR - 03-16-2013, 04:41 PM
RE: insuti testing - jim decker - 03-17-2013, 07:49 PM
RE: insuti testing - CC Solutions - 03-19-2013, 06:41 AM
RE: insuti testing - jim decker - 03-19-2013, 09:35 AM
RE: insuti testing - CC Solutions - 03-19-2013, 08:38 PM
RE: insuti testing - jim decker - 03-20-2013, 07:42 AM
RE: insuti testing - CC Solutions - 03-21-2013, 11:50 AM
RE: insuti testing - CCR - 03-21-2013, 05:08 PM
RE: insuti testing - jim decker - 03-22-2013, 08:45 AM
RE: insuti testing - eaadams - 04-29-2013, 04:27 PM
RE: insuti testing - CC Solutions - 04-29-2013, 07:01 PM
RE: insuti testing - eaadams - 04-30-2013, 09:15 AM
RE: insuti testing - CC Solutions - 05-01-2013, 05:57 AM
RE: insuti testing - CCR - 05-01-2013, 06:16 AM
RE: insuti testing - CC Solutions - 05-01-2013, 06:24 AM
RE: insuti testing - rapidrhrep - 05-01-2013, 10:15 AM
RE: insuti testing - CCR - 05-02-2013, 03:42 AM
RE: insuti testing - CC Solutions - 05-02-2013, 05:53 AM
RE: insuti testing - CCR - 05-02-2013, 06:33 AM
RE: insuti testing - eaadams - 05-02-2013, 08:05 AM
RE: insuti testing - CC Solutions - 05-02-2013, 08:45 AM
RE: insuti testing - eaadams - 05-02-2013, 08:59 AM
RE: insuti testing - CC Solutions - 05-02-2013, 09:02 AM
RE: insuti testing - eaadams - 05-02-2013, 10:21 AM
RE: insuti testing - CC Solutions - 05-02-2013, 11:25 AM
RE: insuti testing - eaadams - 05-02-2013, 11:30 AM
RE: insuti testing - jim decker - 05-02-2013, 12:31 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
Wink article on testing eaadams 3 6,297 09-01-2013, 09:10 AM
Last Post: CC Solutions
  No Testing Requirements ???? CCR 3 5,175 06-28-2013, 10:26 AM
Last Post: eaadams
  Moisture Testing Awareness raised Down Under... Horror abounds... Rubensgt40 6 9,607 05-10-2013, 06:46 PM
Last Post: Rubensgt40
  How Do You Charge For Testing? CCR 23 22,562 03-21-2013, 05:05 PM
Last Post: CCR
  RH & CC Testing CCR 23 41,554 07-26-2012, 06:19 AM
Last Post: CC Solutions
  RH Testing For Parking Garages CCR 6 9,585 07-12-2012, 01:44 PM
Last Post: CCR
  Wood Floor Testing eaadams 1 5,423 06-07-2012, 01:08 PM
Last Post: hnelson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)