Thread Rating:
  • 0 Vote(s) - 0 Average
  • 1
  • 2
  • 3
  • 4
  • 5
creating the hole for the sensor
11-08-2009, 04:17 PM,
#1
creating the hole for the sensor
Sometimes, I find drilling into concrete a a bit of a challenge depending in the slab; some slabs seem harder than others and control of the bit is more difficult. QUESTION: What factors make a hole unsuitable for testing? I've had cases where the depth was right but the sensor would not go in even using the tools and recommended methods; then, after one more (in and out) with the bit, the the sensor went in easily without much effort. If the sensor goes in too eaisly is the hole still usable?
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
creating the hole for the sensor - SDJeff - 11-08-2009, 04:17 PM
RE: creating the hole for the sensor - Ben - 11-09-2009, 04:39 PM