A most unfortunate flooring failure!
12-03-2012, 01:30 PM,
#38
RE: A most unfortunate flooring failure!
Don't get me wrong, I'm not saying all installers have to foot the bill for full ASTM testing. What I'm saying is all installers should be installing at least a few Wagners for their own knowledge.

If I were an installer I sure wouldn't believe anything any testing company told me without a little verification. That could be as little as watching them install the probes. But installing one or two of my own on a little job will either confirm or refute what I was being told.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]