A most unfortunate flooring failure!
11-20-2012, 05:23 PM,
#16
RE: A most unfortunate flooring failure!
Construction budget or not, the installer can protect themselves. But they have to have the nads to do it.

Taking an RH test is easy and inexpensive. Turning down the job may be the best money they ever lost. Wink
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Quote this message in a reply


[-]
Share/Bookmark (Show All)