My contention is that using a cheap test that is close to worthless is more expensive than doing a better test that may cost a tiny bit more initially.

Why not just test the floor by throwing wet chicken feathers at it and seeing how many fall facing due north? I think the same number of flooring manufacturers recognize that test.

The cost of the test is irrelevant if it doesn't provide the results you need to go forward.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Messages In This Thread
Carbide moisture testing - CC Solutions - 09-18-2012, 10:19 AM
RE: Carbide moisture testing - eaadams - 09-18-2012, 11:01 AM
RE: Carbide moisture testing - CC Solutions - 09-18-2012, 12:25 PM
RE: Carbide moisture testing - eaadams - 09-18-2012, 02:02 PM

Possibly Related Threads...
Thread Author Replies Views Last Post
  Moisture going up Rubensgt40 3 1,560 07-05-2014, 03:18 AM
Last Post: Rubensgt40
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,425 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,365 05-19-2014, 10:55 AM
Last Post: eaadams
  Digital moisture meter QC worker 2 1,869 05-10-2014, 08:07 PM
Last Post: Rubensgt40
  Tandus removes moisture testing requirement eaadams 2 4,098 09-27-2013, 10:26 AM
Last Post: eaadams
  RH Testing Thick Slabs CCR 33 48,041 11-21-2012, 10:19 AM
Last Post: eaadams
  Calcium Carbide testing and Silicates Lepito 51 83,178 11-19-2012, 11:59 AM
Last Post: ILLENTINC
  Testing Cost eaadams 22 33,545 07-30-2012, 07:01 PM
Last Post: Ernesto
  Old concrete slab moisture DeanC 23 50,577 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Flooring Manufacturer Warrenty in Relation to Moisture mwoody 5 10,922 08-14-2011, 08:43 PM
Last Post: Ernesto

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)