Calcium Carbide testing and Silicates

#32
(10-21-2012, 04:34 PM)Rubensgt40 Wrote:  
(10-15-2012, 08:34 PM)CC Solutions Wrote:  Hopefully Howard's latest report debunks the silicate myth.....

Yeah, there's only one silicate product down here which is highly promoted in general flooring, I believe it came from the US. It's certainly being pushed as a cure-all for moisture problems. Most adhesive/mitigation manufacturers are highly dismissive of it. That said, there are some concrete coatings producers who warranty over it. Good luck to them.

Of course the adhesive/mitigation manufacturers are highly dismissive of it. It is a competitive product to the standard mitigation systems. When QUALITY products of this nature are PROPERLY used, there is no need for the several dollar a square foot mitigation systems. Do you really think the mitigation manufacturers are going to sing the praises of such a product?
Reply


Messages In This Thread
RE: Calcium Carbide testing and Silicates - ILLENTINC - 11-15-2012, 10:47 AM

Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,482 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  Tandus removes moisture testing requirement eaadams 2 4,132 09-27-2013, 10:26 AM
Last Post: eaadams
  RH Testing Thick Slabs CCR 33 48,263 11-21-2012, 10:19 AM
Last Post: eaadams
  Carbide moisture testing CC Solutions 4 8,709 09-18-2012, 06:11 PM
Last Post: CC Solutions
  Testing Cost eaadams 22 33,710 07-30-2012, 07:01 PM
Last Post: Ernesto
  Mositure Testing Over Concrete Discussion Ernesto 36 68,104 04-19-2011, 04:59 PM
Last Post: CC Solutions
  I offered free RH testing CC Solutions 9 20,539 04-05-2011, 05:33 AM
Last Post: CC Solutions
  RH testing bob huesgen 2 8,569 09-30-2010, 08:27 AM
Last Post: eaadams
  Certified Testing Results Wesley Holley 11 27,291 09-20-2010, 03:01 PM
Last Post: CC Solutions
  Specific humidity or ERH or Calcium Carbide? Andy 11 25,721 05-11-2010, 03:22 PM