I have learned to simply walk away from anything adheared to gypcrete. But do follow the testing guidelines for it we have here. \

The sealers are just as bad if not worse as the ones for concrete because gypcrete can adsorb it more into the top.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Quote this message in a reply


[-]
Share/Bookmark (Show All)
Facebook Twitter Linkedin Technorati Digg MySpace Delicious

Messages In This Thread
Problems in the UK, HELP!!!! - bugs183 - 09-04-2012, 01:42 AM
RE: Problems in the UK, HELP!!!! - Ernesto - 09-04-2012, 07:06 PM
RE: Problems in the UK, HELP!!!! - bugs183 - 09-05-2012, 07:12 AM
RE: Problems in the UK, HELP!!!! - bugs183 - 09-07-2012, 12:01 PM
RE: Problems in the UK, HELP!!!! - Ernesto - 09-08-2012, 12:31 PM
RE: Problems in the UK, HELP!!!! - eaadams - 09-16-2012, 10:45 PM
RE: Problems in the UK, HELP!!!! - eaadams - 09-18-2012, 09:41 AM
RE: Problems in the UK, HELP!!!! - lennyh - 10-02-2012, 04:06 PM